Objective To heat customer-supplied rods of various diameters (0.14 inch to 0.49 inch) to 4170°F (2300°C) at 2-4 feet per minute
Material Tungsten and Molybdenum; Tests are run in an atmosphere of Nitrogen or Hydrogen avoid oxidation of the materials.
Temperature 4170°F (2300°C)
Frequency 100 kHz
Equipment 90 kW, 50-150 kHz solid state induction power supply equipped with a remote heat station containing three,6.6 mF capacitors for a total of 2.2 mF.
An induction-heating coil designed and developed specifically for this application.
Process A multi turn induction heating coil is designed for heating the various rod diameters. An optical pyrometer is used to measure the temperature of the part inside the induction coil.
Initial static tests are conducted, then dynamic tests are run to confirm the results of the static tests.
Results/Benefits 90 kW system heats the rods to temperature at the rate specified. The rods are fixed lengths and are fed individually through the induction coil. The UIHM power supply automatically adjusts output to this varying load in the coil, allowing for an uninterrupted process
Material Tungsten and Molybdenum; Tests are run in an atmosphere of Nitrogen or Hydrogen avoid oxidation of the materials.
Temperature 4170°F (2300°C)
Frequency 100 kHz
Equipment 90 kW, 50-150 kHz solid state induction power supply equipped with a remote heat station containing three,6.6 mF capacitors for a total of 2.2 mF.
An induction-heating coil designed and developed specifically for this application.
Process A multi turn induction heating coil is designed for heating the various rod diameters. An optical pyrometer is used to measure the temperature of the part inside the induction coil.
Initial static tests are conducted, then dynamic tests are run to confirm the results of the static tests.
Results/Benefits 90 kW system heats the rods to temperature at the rate specified. The rods are fixed lengths and are fed individually through the induction coil. The UIHM power supply automatically adjusts output to this varying load in the coil, allowing for an uninterrupted process
Good
Bad
Related Content
Air Cooled clamp coil (half-open coil) for preheating gas pipeline
induction coating by air cooled clamp induction coil
Remove plastic coating from steel tubes by Induction Heating
Releasing Fixture by Induction Heating
U shape air cooled induction coil by UM-100C-HF for pipeline preheating
induction quenching with custom-design inductor
induction brazing diamond segment
induction brass soldering copper plate_2
Hot
induction annealing for stainless pipe
induction annealing umbrella ribs by 60KW induction heater (UM-60AB-UHF)
induction annealing steel wire online
induction annealing steel umbrella ribs by 40KW induction heater (UM-40AB-HF)
induction annealing by horizontal type induction heater
induction annealing rod steel (steel bar)
induction annealing water channel
UHF induction annealing
Newest Comment
No Comment
Post Comment