Objective Heating a steel rod to 1200ºF (649ºC) for an annealing, stress relief application
Material 1.062” (26.97mm) dia type T-410 stainless steel bar 6’ (1.82m) long & 1.25” (31.75mm) dia T-416 stainless steel bar 6’ (1.82m) long
Temperature 1200ºF (649ºC)
Frequency 106 kHz
Equipment • 70kW induction heating system, equipped with a remote workhead containing eight 1.0 μF capacitors for a total of 8.0 μF
• An induction heating coil designed and developed specifically for this application.
Process A two position 8 turn helical parallel coil is used to heat the stainless steel rod for 30 seconds to reach the requested 1200ºF (649ºC).
Results/Benefits Induction heating benefits:
• Process currently done in batch furnaces, induction heating
allows process to be done in-line saving time and energy.
• No rotation of part needed
• Flameless process
Annealing-steel-shaft
Related Content
induction annealing for stainless pipe
induction annealing umbrella ribs by 60KW induction heater (UM-60AB-UHF)
induction annealing steel wire online
induction annealing steel umbrella ribs by 40KW induction heater (UM-40AB-HF)
induction annealing by horizontal type induction heater
induction annealing rod steel (steel bar)
induction annealing water channel
UHF induction annealing
Hot
induction annealing for stainless pipe
induction annealing umbrella ribs by 60KW induction heater (UM-60AB-UHF)
induction annealing steel wire online
induction annealing steel umbrella ribs by 40KW induction heater (UM-40AB-HF)
induction annealing by horizontal type induction heater
induction annealing rod steel (steel bar)
induction annealing water channel
UHF induction annealing
Newest Comment
No Comment
Post Comment